Low carbon alloy Hardness convertor , Hardness convertor , Hardness Convertor for fasteners , HRC, HRA, HRD, HRB ,HB, HV, Tensile strength , Mecanical Pradhan,Hardness, HRB to UTS

Low carbon alloy Hardness convertor , Hardness convertor , Hardness Convertor for fasteners , HRC, HRA, HRD, HRB ,HB, HV, Tensile strength , Mecanical Pradhan,Hardness, HRB to UTS



ii Hardness Conversion Calculator

Hardness Conversion Calculator

Steel & Cast Iron (ISO 18265-2003)~Mechanical Pradhan

Conversion of hardness-to-hardness or hardness-to-tensile-strength values for unalloyed and low-alloy steels and cast iron.Rule ~ Put any value another value automatic appear.

Based on ISO 18265-2003
Valid Range
Tensile strength N/mm² 255 - 2180
Vickers hardness HV10 80 - 940
Brinell hardness HB 76 - 618
Rockwell hardness HRB 41 - 105
Rockwell hardness HRF 82.6 - 115.1
Rockwell hardness HRC 20.3 - 68
Rockwell hardness HRA 60.7 - 85.6
Rockwell hardness HRD 40.3 - 76.9
Rockwell hardness HR15N 69.6 - 93.2
Rockwell hardness HR30N 41.7 - 84.4
Rockwell hardness HR45N 19.9 - 75.4
This application is based on ISO 18265-2003:
Metallic materials, conversion of hardness values.